Application: | Aviation, Electronics, Industrial, Medical |
---|---|
Standard: | GB, ASTM |
Purity: | Mo85cu15 |
Still deciding? Get samples of US$ 120/Piece
Request Sample
|
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
Material | Wt% Molybdenum Content |
Wt% Copper Content |
g/ Density at 20ºC |
W/M.K Thermal conductivity at 25ºC |
(/k) Coefficient of thermal expansion at 20ºC |
Mo85Cu15 | 851 | Balance | 10 | 160-180 | 6.8 |
Mo80Cu20 | 801 | Balance | 9.9 | 170-190 | 7.7 |
Mo70Cu30 | 701 | Balance | 9.8 | 180-200 | 9.1 |
Mo60Cu40 | 601 | Balance | 9.66 | 210-250 | 10.3 |
Mo50Cu50 | 500.2 | Balance | 9.54 | 230-270 | 11.5 |
Material | g/ Density at 20ºC |
(10-6/k) Coefficient of thermal expansion at 20ºC |
W/M.K Thermal conductivity at 25ºC |
||
In-plane | Thru-thickness | In-plane | Thru-thickness | ||
1:4:1 | 9.4 | 7.2 | 9.0 | 340 | 300 |
Class |
Density g/cm3 |
Hardness MN/m2 |
Resistivity μΩ.cm |
Conductivity IACS |
W50Cu50 |
11.85 |
1128 |
3.2 |
54 |
W55Cu45 |
12.30 |
1226 |
3.5 |
49 |
W60Cu40 |
12.75 |
1373 |
3.7 |
47 |
W65Cu35 |
13.3 |
1520 |
3.9 |
44 |
W70Cu30 |
13.8 |
1716 |
4.1 |
42 |
W75Cu25 |
14.5 |
1912 |
4.5 |
38 |
W80Cu20 |
15.15 |
2158 |
5.0 |
34 |
W85Cu15 |
15.9 |
2354 |
5.7 |
30 |
W90Cu10 |
16.75 |
2550 |
6.5 |
27 |